Abstract

For arsenic-containing refractory gold concentrate, gold recovery by leaching is extremely difficult due to the encapsulation of gold in arsenopyrite and pyrite. In this work, the pre-oxidation of a high-arsenic and high-sulfur refractory gold concentrate in the acidic potassium permanganate or hydrogen peroxide solutions has been investigated. The studied parameters include pre-oxidation time, acidity, pre-oxidation temperature, ethylene glycol addition and oxidant concentration. When potassium permanganate of 0.25 mol/L is used as oxidant, 61.4% of arsenic and 51.8% of iron can be removed, respectively. The results of kinetics analysis indicate that the oxidative dissolution of arsenopyrite during the pre-oxidation process is controlled by the product layer diffusion, with an activation energy of 7.92 kJ/mol. The stability of hydrogen peroxide can be significantly improved by increasing both sulfuric acid concentration and ethylene glycol addition when hydrogen peroxide is used as oxidant. Under optimum conditions, arsenic removal ratio of 57.2% and iron removal ratio of 51.9% have been achieved with hydrogen peroxide of 2.5 mol/L, sulfuric acid of 0.75 mol/L and ethylene glycol of 30 mL/L. The gold extraction of refractory concentrate is only 11.5% in the copper–ammonia–thiosulfate leaching solutions without pre-oxidation. A gold extraction of 71.8% and significant decrease in thiosulfate consumption from 28.2 to 5.7% have been observed for the concentrate after pre-oxidation.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call