Abstract

The pressure-less sintering of slag α-Sialon powder, derived from slag wastes by self-propagating high-temperature synthesis technology, was carried out and the phase assemblages of slag α-Sialon sintered at different temperatures were studied. The results showed that the formation of β-Sialon phase did occur during the pressure-less sintering and was restrained to some extent via mass diffusion of Ca2+/Mg2+ added in embedded powder in samples. α-Sialon phase with two different unit cells was detected in samples sintered at 1700°C and above, and the formation mechanism was also discussed.