The paper analyzed the martensite transformation characteristic of Fe-Mn-Si alloy by XRD analysis and tensile test under different deformation condition. In this study, the amount of ε martensite of Fe-17Mn-5Si-10Cr-5Ni alloy was lower than that of Fe-17Mn-5Si-2Cr-2Ni-1V alloy under the same deformation condition, but the change rate of ε martensite was much higher than that of Fe-17Mn-5Si-2Cr-2Ni-1V alloy, and the stress relaxation rate of the both alloys increased with the increase of the stop loading time, and the relaxation rate of the Fe-17Mn-5Si-10Cr-5Ni alloy was obviously higher than that of Fe-17Mn-5Si-2Cr-2Ni-1V alloy. ()

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.