Titanium alloy Ti6Al4V has been widely applied to medical, automotive, and aerospace industries due to its excellent properties such as high strength and excellent corrosion resistance. On the other hand, additive manufacturing (AM) technology can give the freedom of design of the products. In order to spread the AMed products, the joining of AMed and wrought products are required, and it is important to understand the joint characteristics. In this study, butt welding of Ti6Al4V plate was conducted by fiber laser in argon shielding, and the joint characteristics of laser weld wrought/wrought, AMed/AMed, and AMed/wrought Ti6Al4V plates were experimentally investigated. The AMed plate has higher tensile strength than wrought plate but the elongation of AMed plate is smaller, since AMed plate has α’ martensite due to rapid cooling during laser irradiation in AM process. Then, the laser weld joint of AMed/AMed plates has higher tensile strength, but smaller elongation than that of wrought/wrought plates. The weld joint of AMed/wrought plates shows good welding state, since small heat input leads to formation of small weld bead with higher hardness between wrought and AMed plates.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.