Abstract

The joints of RSW for HSHSS were prepared with IF spot weld equipment. The weld nugget, fracture mode, microstructure and micro-hardness of the joints were investigated. The weld nugget increases and the fracture mode changes from interfacial fracture to nugget plug fracture with the increasing welding current. There are three distinct zones in the weld joint: weld nugget, heat affected zone (HAZ) and base metal. The microstructure of HAZ includes tempered zone (HAZ-1), incomplete quenching zone (HAZ-2) and complete quenching zone (HAZ-3). The micro-hardness of weld nugget and HAZ-3 is same with the base metal. The micro-hardness of HAZ-1 and HAZ-2 is smaller than that of base metal.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.