This work makes an attempt to study of fracture behaviour of hybrid Composite reinforced with hard ceramic Boron carbide as primary phase and secondary phase as soft solid lubricant Molybdenum Disulphide with base matrix Al2219 by two stage stir casting method is incorporated. Compact tension type specimen was utilized for test and dimensions are conformity to ASTM E-647.Fatigue crack growth and fracture toughness test conducted as per ASTM Standard E-399 and E-1820. This study discloses that reinforcing the hard ceramic Boron Carbide of constant 3wt% and soft solid lubricant Molybdenum Disulphide with increasing wt% of 3%, 4%, 5% to Al2219, results increase in energy required to open the crack front to create two new crack surfaces during mode-I type failure and also significantly variation of fracture toughness. Surface of fractured specimens were study under scanning electron microscope and observes that pulled regions tiny dimples results in balance between ductility and strength of prepared hybrid composite.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.