Abstract

Although the transverse butt weld method with ceramic backing strip has been widely used in various industrial fields for its fabricational convenience, it is rarely used in offshore industries since the fatigue strength of the weld joint has not been proved sufficiently. This study conducted fatigue tests for series of butt weld specimens with horizontal (2G) and vertical (3G) welding positions in order to verify the fatigue strength compared to S-N curve by DNV (Det Norske Veritas), IIW (International Institute of Welding) and Eurocode 3. The difference of the 2G specimens and the 3G specimens are investigated in terms of angular distortion and the effect on the fatigue strength are analyzed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.