The fatigue crack growth behavior of weld metal (WM), heat affected zone(HAZ) and base metal(BM) of Duplex Stainless Steel 2205(DSS) has been determined at high-frequency fatigue testing machine. The results show that the fatigue crack growth rate of WM is slowest and the ability to resist fatigue crack growth is highest in the three parts. Secondly, the sensitivity caused by the stress change of WM is the highest, followed by HAZ, and the BM is the weakest.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.