Abstract

A fabrication process to manufacture SU8 photoresist microstructures is presented in which BP212 positive photoresist was used as sacrifice layer and SU8 was used as structure layer. No crack has been observed in the obtained microstructures. The relation between PEB temperature and stress gradient in SU8 film has been studied by measuring radii of released SU8 cantilevers made at different PEB temperatures.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.