In this study, the interactions between Ni and YSZ in solid oxide fuel cell anode and the influence of glass seal to anode performances have been investigated by pure Ni anode sintered on YSZ pellet. The evolution of Ni–YSZ interface in 100h galvanostatic polarization in hydrogen is studied with different humidities in hydrogen. Electrochemical impedance spectroscopy was applied to analyze the time variation of the anode electrochemical characteristics. The interface microstructural changes were characterized by scanning electron microscopy. The influence of bulk gas humidity, gas-sealing material and Ni coarsening on anode durability was studied. The degradation of pure Ni anode is considered to be determined by the competition among the mechanisms of silicon deposition, YSZ interface morphological change and Ni coarsening.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.