ABSTRACT The mulberry fiber is extracted from the mulberry bast by biochemical degumming method. Based on the single factor experiment, the orthogonal experiment is further designed. The optimal process parameters for biochemical combined degumming are as follows: pretreatment stage, sulfuric acid solution concentration 2.5g/L, time 1h, temperature 60°C, bath ratio 1:20; alkaline pectinase treatment stage, alkaline pectinase solution concentration 46g/L, time 8h, temperature 50°C, bath ratio 1:20, solution pH = 9; alkali boiling stage, sodium hydroxide solution concentration 10g/L, alkali boiling time 3h, sodium silicate 30g/L, temperature 100°C, bath ratio 1:20; xylanase treatment stage, the concentration of xylanase solution 9g/L, the time 4h, the temperature 50°C, the bath ratio 1:20, and the solution pH = 4.8. By comparing the properties of mulberry fiber obtained by biochemical degumming and chemical degumming, it is found that the biochemical degumming process has less damage to fibers and more effective removal of lignin and hemicellulose.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.