Zr–2.5Nb and Excel pressure tubes, both containing α and β phases were submitted to different heat treatments. Then, hydrogen Terminal Solid Solubility for Dissolution (TSSD) and Precipitation (TSSP) curves were measured by Differential Scanning Calorimetry (DSC). The solvus of Excel heat treated at 380 °C–24 h or 750 °C–0.5 h exceeds the solvus of Zr–2.5Nb in standard conditions of CANDU pressure tubes. Aging at 500 °C–168 h decreases the limit of solubility. The lowest solubility was obtained in Excel aged at 500°C–168 h. In DSC measurements the effect of maximum temperature and hold time at such temperature on solubility curves were studied. The TSSD decreases when thermal cycle causes decomposition of the β phase, and is recuperated when α → α + β transformation temperature is exceeded. The TSSP is affected not only by βZr phase decomposition but also by the relief of defects produced during hydride precipitation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.