Abstract
Differential scanning calorimetry (DSC) thermal analysis is a well-accepted technique used to measure the transformation temperatures of shape memory alloy and its thermoelastic transformation energies. In this study, both forward and reverse transformation temperatures of a nickel-free Ti-19Nb-9Zr (at.%) SMA were investigated using DSC technique with different cooling and heating scanning rates in a range of 10 to 100 °C/min. The results showed that the transformation temperature intervals vary substantially with respect to the thermal scanning rates. It is found that the martensitic start (Ms) temperature decreases with decreasing the cooling rates. The optimal scanning rate was found to be 40 °C/min for obtaining the maximum thermoelastic transformation energies stored between the forward and the reverse martensitic transformations. It is believed that the thermoelastic transformation energy increases with the increase in the volume fraction of martensite. Based on these measurements, these thermoelastic transformation energies between the forward and the reverse martensitic transformations were estimated to be ~21 and ~27 J/g, respectively. The appropriate selection of scanning rate for SMA analysis will be discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.