Abstract
Differential absorption spectra of RbAg4I5 have been measured in the exciton absorption region of AgI within the temperature range 27–250 °C. In the same temperature range, the temperature behavior of the heat capacity of RbAg4I5, Rb2AgI3, and KAg4I5 have been obtained by differential scanning calorimetry. An analysis of the results suggests that, in AgI microcrystals less than rcr in size, the upper boundary for stability of the low-temperature β modification is higher by several tens of degrees.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.