Abstract

Ni + Mo composite coatings were prepared by electrodeposition of nickel from a nickel bath containing Mo particles suspended by stirring. All the coatings have been deposited under galvanostatic conditions. It was found, that molybdenum content depends on the deposition current density and changes between 28 and 46 wt%. The thickness of the Ni + Mo composite coatings was between 100 and 130 μ m depending on the deposition current density. Ni + Mo coatings were characterized by larger surface area than the Ni electrodeposits. Structural investigation carried out by X-ray diffraction (XRD) method show that the obtained coatings consist of crystalline Mo phase incorporated into Ni matrix. The apparent and intrinsic coating activity and the mechanism of the hydrogen evolution reaction (HER) were studied by electrochemical impedance spectroscopy (EIS) and steady-state polarization methods. The results demonstrate greater apparent activity of Ni + Mo composite coatings towards hydrogen evolution in comparison with pure Ni matrix. For the Ni + Mo composite electrodes, increase of the amount of molybdenum particles embedded into Ni matrix causes simultaneously important increase in the apparent activity, increase in the electrochemically accessible surface area, and a small decrease in the intrinsic activity.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.