Abstract

In this work, the results of the characterisation of an electroless brass film deposited on low carbon steel are correlated with the conditions of application of an intermediate zinc film. The results report that the best conditions of electroless brass plating are obtained when the zincate is done under current density of 7–10 A/dm², temperature of 40°C and with immersion time of 35–45 seconds.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.