Abstract
Coal, iron and manganese ore samples were exposed to different ultrasonic intensities of 250, 300 and 350 W/L for five minutes and to an ultrosonic intensity of 270 W/L for different time durations of 3, 5 and 7 minutes. The ultrasonically treated samples showed reductions in D80 particle diameters of 6 percent for the coal samples, 5.95 percent for the iron ore samples and 35.63 percent for the manganese ore samples during grinding. The ultrasonic treatment was also observed to assist in reducing ash content in the coal product by 8 percent and to reduce manganese losses in rejects by about 5 percent. Ultrasonic treatment was concluded to be capable of assisting in the comminution of friable ores more prominently than the hard and porous materials.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.