Abstract
This paper presents the results of studying the production of molybdenum-tungsten alloys by spark plasma sintering at various process conditions, as well as the processes of material compaction and structure formation. A comparative analysis of compactability of molybdenum-tungsten alloys produced by spark plasma sintering and sintering in hydrogen was performed. It was shown that a relative density of > 95% can be achieved at a temperature of 1,800°C and external pressure of 50 MPa.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.