Abstract

AbstractMolecular orientation in poly(ethylene terephthalate) (PET) fibers was studied by polarized fluorescence. The observed amorphous orientation of the spun as fiber was not random but uniaxial along the fiber axis. This orientation increased with draw ratio up to about 2 and then remained fairly constant. The amorphous regions of PET fibers were disoriented when the fibers were heated while unconstrained. The fluorescence data obtained were correlated with shrinkage measurements. Fluorescence data indicated that spin drawing had more effect upon orientation than subsequent drawing of the fiber, whereas birefringence data indicated the opposite. The reason for this behavior is discussed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.