Abstract

Single-phase samples of orthorhombic YFe1−xMnxO3 (x = 0 to 0.3) were prepared using solid-state route. Temperature variation of magnetization measurements show antiferromagnetic transition with Neel temperature (TN) in the range of 646 K for x = 0 to 456 K for x = 0.3. Spin canting-induced weak ferromagnetism is observed for T < TN. These materials exhibit an exchange bias behavior as per magnetic hysteresis loop measurement under field-cooled condition. The magnitude of maximum exchange bias field at 413 K is around 1.2 kOe. The observed exchange bias is explained by considering the exchange coupling across the interface of two magnetic phases having a dominant collinear antiferromagnetism and a weak ferromagnetism, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.