Abstract
23Nov 2016 STUDY OF CASTING DEFECTS AND THEIR REMEDIES – A REVIEW. Rashi P.Gaikwad and Pankaj A. Gaikwad. Assistant Professor, Mechanical Engineering, Indira College of Engineering, Pune. Manager, Bajaj Auto Limited, Pune.
Highlights
During this process there are different critical factors which is contributing in large amount to the defects
Received: 25 September 2016 Final Accepted: 27 October 2016 Published: November 2016 today is the first step in manufacturing most product. In this process the material is first liquefied by proper heating and this liquefied is poured into a previously prepared mould cavity where it is allowed to solidify and subsequently the product is taken out, cleaned and trimmed to the required shape
Casting is the one of the oldest manufacturing processes, and even today is the first step in manufacturing most product
Summary
Received: 25 September 2016 Final Accepted: 27 October 2016 Published: November 2016 today is the first step in manufacturing most product In this process the material is first liquefied by proper heating and this liquefied is poured into a previously prepared mould cavity where it is allowed to solidify and subsequently the product is taken out, cleaned and trimmed to the required shape. Casting is the one of the oldest manufacturing processes, and even today is the first step in manufacturing most product