Al-Ca master alloy was prepared by molten salt electrolysis method, using a mixed molten salt system of CaCl2-CaF2and feeding CaO as electrolysis material. The technological parameters such as back electromotive force (BEMF), cell voltage, and current were measured by testing device of molten salt electrolysis. The effects of current density, CaO addition, electrolysis time and feeding period on the back electromotive force in the electrolysis process are studied. The results indicate that back electromotive force increases with current density increasing, the feeding period is 30min measured by potential control method. Finally, the Al-Ca alloy with the Ca content of 11.6wt% can be obtained by electrolyzing for 1h at the current of 7A and at 740.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.