Abstract

We present the strand and formed method of manufacturing Ag-sheathed Bi-system superconducting round wire. The method strands three round multifilamentary wires into a single round wire. For the strand and formed Bi2Sr2Ca1Cu2Ox (Bi-2212) wire, the critical current Ic exhibited almost no change until the bending strain exceeded 0.6%, while for the conventional round Bi-2212 wire Ic deteriorated when the bending strain exceeded 0.2%. Also, we have measured the alternating-current transport loss of both a strand formed round Bi-Pb2Sr2Ca2Cu3Ox (Bi-2223) wire with a barrier and a conventional tape Bi-2223 wire without a barrier. The measured loss normalized by the Ic of the former was more reduced than that of the latter.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.