Abstract

To improve the accuracy of polymer interfacial tension measurement using deformed drop retraction method (DDRM), we examined some factors, such as the shape parameter, the retraction scale D 0, and the distortion criterion γ by means of dissipative particle dynamics (DPD) simulation with 6 different models and analysis with three observation data, and proposing a new shape parameter P. Results show that the shape parameter order of suitable to various retraction scales and larger distortion is P>( a 2− b 2)> D. This study found that choosing a suitable retraction scale is very important, and that D 0≅0.15 is the most suitable retraction scale in DDRM measurement. In the scale, the three shape parameters cannot make much difference on the measurement deviation from the standard. This study also found that the distortion criterion γ varies with different shape parameters. We also found here when D 0≅0.15 the distortion criterion becomes γ<0.15, and one has a reliable measurement with any shape parameter.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.