Abstract

The effect of heat treatment on the Fe 2+/Fe 3+ ratio in some alkali phosphate glasses containing antimony and iron oxides has been investigated. Differential thermal analysis, Mossbauer spectroscopy, magnetic susceptibility and density measurements as well as the molar volume calculations were used in this study. The obtained data indicate that all glasses show approximately unchangeable stability. It is found, from the area under the Mossbauer absorption spectra that ferrous transformed gradually to ferric ions and the transformation rate constant was found to be 48 min −1. The elapsed time was found to be 160 min. This transformation represents a first-order solid state reaction. The molar magnetic susceptibility measurements confirm the above results.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.