The use of a tantalum wire in hot-wire chemical vapour deposition (HWCVD) has allowed the deposition of dense nanocrystalline silicon at low filament temperatures (1550 °C). A transition in the crystalline preferential orientation from (2 2 0) to (1 1 1) was observed around 1700 °C. Transmission electron microscopy (TEM) images, together with secondary ion mass spectrometry (SIMS) measurements, suggested that no oxidation occurred in materials obtained at low filament temperature due to the high density of the tissue surrounding grain boundaries. A greater concentration of SiH 3 radicals formed at these temperatures seemed to be responsible for the higher density.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.