Abstract

According to the principle of ultrasonic vibration turning, the first step is to study different position changes of surface roughness with cutting parameters under ultrasonic vibration turning of slender shaft by the test of single factor, and determining the extreme position of surface roughness with the slender shaft changes in different cutting conditions. The second step is to study the influence of cutting parameters on the overall average surface roughness of work piece under ultrasonic vibration turning of slender shaft by orthogonal test design, and compared with the conventional turning. The experimental results show that ultrasonic vibration turning slender shaft processing can significantly improve the surface roughness. At the same time, the influence laws of cutting parameters on the surface roughness are investigated, and finding out the optimal cutting experimental parameters.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.