Abstract

One kind of Chinese waste tire's sample was pyrolyzed under an inert atmosphere by using thermo-gravimetric apparatus (TGA) and differential thermal analysis (DTA). Different pyrolysis temperature ranges were determined according to the reaction transition temperature obtained by TGA and DTA. Then, at each temperature range, the pyrolysis gaseous products were analyzed by gas chromatography (GC). The influence of the temperature range on the relative yields of the major decomposition products is studied, and a mechanism for the formation of the main components was also investigated. The results indicate that pyrolysis of waste rubber follows the radical mechanism, and the major products are not seriously affected by increasing the temperature from room temperature to 420 °C and from 421 to 600 °C, but the degradation of blend rubber is different for each of the compositional elastomer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.