Abstract

Modes for heat treatment for homogenizing the cast structure and raising the processibility of alloy AA2014 are determined by empirical methods with the use of light microscopy. The time and temperature of annealing, which determine minimization of dendritic segregation and dissolution of particles of secondary phase, are chosen for a typical commercial ingot. Homogenization at 500°C for 26 h is chosen for alloy AA2014 (the Russian counterpart is AK8) with a mean grain size of 200 μm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.