To investigate the struvite precipitation under constant and non-constant pH conditions and to test a stainless steel device under different operating regimes to maximize the recovery of struvite. The molar ratio of NH4+: Mg2+: PO4(3-) was adjusted to 1: 1.2: 1.2 and pH was elevated to 9.0. The absorbance measurement was used to trace the process of struvite crystallization. Wastewater and precipitate analysis was done by standard analytical methods. The pH constant experiment reported a significantly higher struvite precipitation (24.6 +/- 0.86 g) than the non-constant pH experiment (19.8 +/- 1.86 g). The SAR ranged from 5.6 to 8.2 g m(-2) h(-1) to 3.6-4.8 g m(-2) h(-1) in pH constant and non-constant experiments, respectively. The highest struvite deposit on the device was found in regime 3 followed by in regimes 2 and 4. The highest PO4(3-) (97.2%) and NH4+ (71%) removal was reported in the R1 regime. None of the influent Cu2+ or Zn2+ was precipitated on the device. A higher struvite yield is evident in pH constant experiments. Moreover, the stainless steel device facilitates the isolation of heavy metal free pure (around 96%) struvite from swine waste biogas digester effluent contaminated with cu2+ and Zn2+ and the highest yield is attainable with the device operating at 50 rpm with agitation by a magnetic stirrer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.