Abstract
There were carrying out investigations of processes of structuring and phase formation during receiving of composite ionic-plasma vacuum- arc nano crystal coatings TiN–Ni in broad interval of concentrations of nickel (from 0 to 26 at.%). There was defined that introduction of Ni into composition of coating leads to milling of crystallites of nitride phase. Average grain size of TiN reduced from 100–120 to 15–18 nm under alteration of concentration Ni from 0 to 12 at.% and normal distribution pf grain size. Further increasing of Ni composition accompanied with transition to polymodal distribution of particles with increasing of average diameter up 27 nm for tertiary mode. At concentration of Ni up 12–13 at.% nickel in coating is in X -ray amorphous state. Under it increasing more than 13 at.% in the composition of coating is formed intermetallide TiNi. This, in turn, stipulated appearance of porosity in the structure of deposited layer. Simultaneously with formation of intermetallide decreasing blocking role of nickel, and this is appeared in the growth of single grains of TiN up 30–35 nm. Coatings TiN–Ni are characterized by thermal stability of structure and composition at heating up 800 °C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Izvestiya Vuzov. Poroshkovaya Metallurgiya i Funktsional’nye Pokrytiya (Proceedings of Higher Schools. Powder Metallurgy аnd Functional Coatings)
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.