Abstract

Herein, the x(NaBi)0.5MoO4-(1-x)Bi2/3MoO4 (xNBM-(1-x)BMO, x = 0.2 ∼ 0.8) microwave dielectric ceramics with low sintering temperatures were prepared via the traditional solid-state method to adjust the τf value and dielectric constant. The crystal structure was determined using X-Ray diffraction and Raman spectroscopy, the microstructure was investigated using scanning electron micrograph and energy disperse spectroscopy, and the dielectric properties were studied using a network analyser and infrared spectroscopy. For the xNBM-(1-x)BMO composite ceramics, the (NaBi)0.5MoO4 tetragonal phase coexisted with the Bi2/3MoO4 monoclinic phase. With the rise of x value, the permittivity increased from 23.7–29.8, and the τf value shifited from -53.3 ppm/°C to -13.7 ppm/°C. The 0.8NBM-0.2BMO ceramic sintered at 680 °C possessed excellent microwave dielectric properties with a εr = 29.8 (6.7 GHz), a Qf = 11,800 GHz, and a τf = -13.7 ppm/°C. These results made the xNBM-(1-x)BMO composite ceramics great candidates in low temperature co-fired ceramics technology.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call