AbstractThe blend materials from waterborne polyurethane (WPU)/starch (ST) with different contents (10–90 wt %) were satisfactorily prepared by using the solution casting method. Their miscibility, structure, and properties were investigated by wide‐angle X‐ray diffraction (WAXD), scanning electron microscope (SEM), different scanning calorimetry (DSC), dynamic mechanical thermal analysis (DMTA), and the tensile tests, respectively. The results indicated that tensile strength of composite materials not only depended on the starch content, but also related to the microstructure of WPU. The sample WPU2 (1.75 of NCO/OH molar ratio) exhibited hard‐segment order, but WPU1 (1.25 of NCO/OH molar ratio) had no hard‐segment order. The appropriate starch filled into WPU not only decreased the ordered region of soft‐segment matrix, but also hindered the formation of hard‐segment ordered structure. The blend material from 80 wt % WPU1 and 20 wt % starch exhibited better tensile strength (27 MPa), elongation at break (949%), and toughness than others. With an increase of starch content, the WPU matrix with dispersed starch in the blends transited to dual‐phase continuity and then to starch matrix with dispersed WPU. The results suggested that a certain extent of miscibility existed between WPU and starch in the blend materials on the whole composition ratio. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 90: 3325–3332, 2003
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.