Abstract

The microstructure, phase composition, and room-temperature mechanical properties of the corrosion-resistant Fe-20pctCr-5pctV alloy doped with nitrogen by high-temperature gas-phase nitriding under different conditions have been investigated. The nitriding of the Fe-20pctCr-5pctV alloy at T = 1223 K to 1373 K (950 °C to 1100 °C) and subsequent annealing at T = 973 K (700 °C) lead to the precipitation of large vanadium nitride and disperse chromium nitride particles in the ferrite matrix. Such a treatment increases the strength of the Fe-20pctCr-5pctV alloy at room temperature by 1.6 times, while maintaining the adequate relative elongation. The alloy in the initial state and after nitriding is highly resistant to corrosion.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.