Abstract BaCe 0.7 Y 0.2 In 0.1 O 3–δ (BCYI) compositions were prepared by a modified Pechini method, following this the ceramic samples were consolidated using conventional sintering (CS) and spark plasma sintering (SPS) at 1250–1500 °C for 3–10 min. The structural and microstructural characteristics of the samples were determined using XRD, SEM and TEM. The total, bulk and grain boundary ionic conductivities were evaluated using the AC impedance method in dry air, wet air and dry Ar. It was shown that application of SPS in case of nanocrystalline BCYI allows to reduce the sintering time, and in case of microcrystalline BCYI application of SPS after CS allows to improve hardness and total conductivity through reduction of grain boundary resistance.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.