Abstract
Silver-containing high-silica glasses were synthesized by an impregnation of the silica porous glasses (PGs) first with AgNO3 aqueous solution (with or without the presence of the sensitizers, such as Cu(NO3)2 or Ce(NO3)3), next in the mixed halide salt (NH4Cl, KBr, KI) solution. Then some part of the samples was sintered at the temperatures from 850 to 900°C up to closing of the pores. The structure of glasses was studied by UV-VIS-NIR and IR spectroscopy and X-ray diffraction (XRD) techniques. According to XRD data the silver-containing high-silica glasses contain the AgBr, AgI, Ag3PO4, (CuBr)0.75(CuI)0.25 phases. IR spectra confirmed B-O-B, Si- O-Si, P-O-P, O-P-O, O-B-O bonds, (PO4)3- and P-O- groups in glasses.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.