Abstract
In this search structural, optical and electrical properties were studied by preparing a sample of lead iodide applied to glass bases by thermal evaporation process. The film showed a hexagonal crystalline shape. The value of the energy gap for a sample of 200 nm thickness is 2.9051 eV the intensity is at the plane (003) it’s equal 12.5 nm in this research the value of the energy gap was (2.15eV-2.33) eV and the electrical properties were studied for a sample of. The measurements were made for the electrical conductivity, mobility, carrier’s concentration and finally the Hall coefficient. The results are (1.038*10-5, 0.6727*10+2, 1.009*1012 and 2.631*106) respectively
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.