Abstract The duplex treatment of nitriding and TiAlN coatings was employed to improve the wear resistance of the Ti6Al4V alloy at higher temperature. Mechanical properties, microstructure and high temperature tribological behaviors were investigated by ball-on-disc wear test at elevated temperatures from 25 °C to 600 °C in atmosphere. The duplex treated sample exhibits a superior adhesion compared with only TiAlN coated sample due to a good load-carrying capacity. In addition, the duplex treated sample possesses excellent abrasion resistance at all temperatures. Particularly, the duplex treated sample has the lowest wear rate at 500 °C due to the formation of Al 2 O 3 and TiO 2 .

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.