Carbonaceous deposits (hard coke) were studied by various solid state 13C nuclear magnetic resonance (NMR) techniques after demineralization of the spent and regenerated fluid catalytic cracking (FCC) catalysts obtained from Indian refineries. A number of structural parameters such as aromaticity, H/C ratio, fraction of protonated (faP) and non-protonated (faNP) aromatic carbons, number of pericondensed rings per average molecule (Nperi), and aromatic condensation index (γar) are derived from the NMR data. Findings of thirty-two and thirty-nine aromatic rings in coke from regenerated catalysts and five and nineteen rings in coke from spent catalysts are rationalized by various parameters such as feed, temperature and process conditions of FCC reactor on the basis of condensation. The coke are found more condensed in regenerated catalysts compared to spent catalysts revealing that the temperature has a marked effect in the evolution of coke structure whereas feeds and other process conditions govern the nature and composition of coke.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.