Abstract

Porous sulfated zirconia foams were manufactured by a simple methodology based on the sol–gel process combined with a liquid foam template that used a surfactant mixture. A block copolymer (Pluronic F-127) and an anionic surfactant [sodium dodecylsulfate (SDS)] were mixed in different proportions in order to optimize the porous and surface properties of the ceramic material. By adjusting the SDS/Pluronic ratio, it was possible to obtain sulfated zirconia with a combination of macropores and mesopores that provided high porosity (≈90 %) and surface area (≈80 m2 g−1). The sulfate groups linked to the zirconia surface stabilized the tetragonal phase, to the detriment of the thermodynamically stable monoclinic phase. The sulfate groups and the tetragonal phase decreased as a function of the amount of SDS in the liquid foam template. The combined porous and structural characteristics, together with surface acidity, provided enhanced catalytic activity when the sulfated zirconia foams were employed in the isopropanol dehydration reaction. A further benefit was the selectivity towards propene and negligible formation of acetone.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.