Abstract

The effect of continuous laser irradiation (λ = 1.06 μm) with laser power of 45 W on the structure of Fe73.5Nb3Cu1Si15.5B7 amorphous alloy has been studied using X-ray diffraction and SEM methods. The sample of the ribbon has been placed at a distance from the focal plane of the lens, so a laser beam has been defocused and the diameter of laser spot on the ribbon surface has been about 10 mm. An exposure time τ varied within interval 0.25–0.70 s. Under such conditions structural transformation processes, which depend on the exposure time, have occurred in an irradiated zone. Crystallization process has started at τ = 0.35 s with the formation of α-Fe(Si) nanocrystalline phase, while complete crystallization has occurred at τ = 0.55 s with formation of two nanocrystalline phases: α-Fe(Si) and a hexagonal H-phase.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.