In this work, CdSe thin films have been prepared by chemical bath deposition on glass substrates using and as a source of and respectively, with a solution concentration 0.5M, a solution temperature at 70oC, pH=9 and deposition time 3 hours. The doping process was carried out with tin Sn and copper Cu with different amounts 0.5%, 1%, 1.5% also by CBD. The XRD studies show that the pure and the doped thin films were polycrystalline and cubic structure in the (111) plane direction, (220) and (311) too. SEM technique used to identify the surface nature of CdSe thin films as well as the average crystal size of the growing grains was (5.9nm). The images show a spherical grain, microcode, and other floral shapes with Cu doping at 70oC.

Highlights

  • CdSe thin films have been prepared by chemical bath deposition on glass substrates using

  • ‫يمكن تشخيصها في طيف الحيود الأغشية المشوبة بالنحاس والمحضرة بدرجة ح اررة ترسيب ‪.70oC‬‬ ‫وقد بينت د ارسة سطح غشاء ‪ CdSe‬بتقنية ‪ SEM‬ظهور عناقيد من حبيبات كروية الشكل متجانسة ومنتشرة وملتصقة بشكل‬ ‫جيد على السطح في الأغشية النقية وتصبح اكثر بلورية وتجانسا في الأغشية المشوبة‪ ،‬فضلا عن ظهور عصيبات دقيقة واشكال‬ ‫زهرية في الأغشية المشوبة بالنحاس والمحضرة بهذه الدرجة‪ .‬كما ان الحجم البلوري ينقص بزيادة نسبة التشويب عموما بعد أكثر‬ ‫من ‪ ،1%‬وعلى الرغم من ظهور اشكالا مختلفة عند التشويب بالنحاس والتي قد تكون ظهرت عرضياً في مثل هذه الظروف‪ ،‬الا‬

Read more

Summary

Introduction

‫الخصائص التركيبية للأغشية المشوبة ‪ CdSe:Cu‬و‪CdSe:Sn‬‬ ‫والمحضرة بتقنية الحمام الكيميائي عند درجة ح اررة ‪70oC‬‬ ‫‪ SEM‬للتعرف على طبيعة سطح أغشية ‪ CdSe‬وكذلك معدل الحجم البلوري للأغشية‬

Results
Conclusion
Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call