Abstract
Indium sulfide Nano layers on glass substrate was prepared by Chemical Bath Deposition (CBD) method, at different deposition temperatures 30˚C and 70˚C for about 45 minutes as deposition time. Crystalline and Nanostructures of the layers were obtained, by using X-ray Diffraction (XRD) and Atomic Force Microscopy (AFM) analysis.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.