Multi-phase ternary oxide glass thin films of potassium antimony oxide were synthesized via dip coating (DC) and spray pyrolysis (SP) methods. The growth of thin film was conducted on a non-conductive borosilicate glass substrate. Surface morphology was investigated and showed different characteristics. X-ray diffraction (XRD) analysis revealed the peaks corresponded to the monoclinic KSb3O5 and K2Sb4O11 phases. The structural parameter analysis shows that the lower values of micro strain (ε), dislocation density (δ), and stacking fault probability (SF) with higher number (N) of particle in the multi-phase thin film for the spray pyrolysis method confirm slightly larger crystallite size, less crystal imperfection, and less structural disorder. The lower average transmission, absorption, and extinction coefficients resulted to higher refractive index, permittivity, and electrical susceptibility for the sample synthesized by a spray pyrolysis method. In addition, the average energy band gap values (Eg) of 3.57 and 3.60 eV were obtained for the dip coating and spray pyrolysis methods, respectively. However, the lower Rs (14.69 × 107 Ω/sq.) with higher σh (85.09 S/cm) and the FOM(H-HR) (0.183 Ω-1) of the multi-phase K–Sb–O thin film for the dip coating method were obtained may be due to more interconnections generated at the interface and there are less residual on the surface of thin film.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.