Chemical Spray Pyrolysis (CSP) method is employed to deposit CdS and Silver (Ag)-doped CdS films. The effect of Ag doping at 1, and 3 wt-% levels is considered. The principal X-ray diffraction peak was along (020) plane. Maximum grain size was observed at the (CdS:3% Ag) films. The dislocation density parameter increased from 53.04 to 37.08, whereas the strain(%) parameter decreases from 25.23 to 21.10. Atomic force Microscope (AFM) images indicate a polycrystalline structure, and reveal that the undoped CdS and doped CdS:Ag films have discontinuous surfaces with spherically grains decreased from (58.05 to 45.77 nm) with the increase of doping from 0% to 3%. Root-mean square (Rrms) roughness of surface is about (9.81-5.42) nm. Also, there was a clear decrement in transmittance as Ag increment. The optical energy bandgap Eg has been decreased from 2.47 to 2.37 eV due to increase in Ag content. The absorption coefficients with photon energy increase with increasing concentration doping in Ag.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.