Abstract

The structural properties of Pt films grown by atomic layer deposition (ALD) are investigated with synchrotron based x-ray scattering and x-ray diffraction techniques. Using grazing incidence small angle scattering, we measure the lateral growth rate of the Pt islands to be 1.0 Å/cycle. High resolution x-ray diffraction reveals that the in-plane strain of the Pt lattice undergoes a transition from compressive strain to tensile strain when the individual islands coalescence into a continuous film. This transition to tensile strain is attributed to the lateral expansion that occurs when neighboring islands merge to reduce their surface energy. Using 2D grazing incidence x-ray diffraction, we show that the lattice orientation becomes more (111) oriented during deposition, with a sharp transition occurring during coalescence. Pt ALD performed at a lower deposition temperature (250 °C) is shown to result in significantly more randomly oriented grains.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.