The objective of this study was to fabricate dual‐layer hollow fiber as a microreactor for potential syngas production via phase inversion‐based co‐extrusion/cosintering process. As the main challenge of phase inversion is the difficulty to obtain defect‐free fiber, this work focuses on the effect of the fabrication parameters, that is, nonsolvent content, sintering temperature and outer‐layer extrusion rate, on the macrostructure of the produced hollow fiber. SEM images confirm that the addition of nonsolvent has successfully minimized the finger‐like formation. At high sintering temperature, more dense hollow fiber was formed while outer‐layer extrusion rate affects the outer layer thickness.