The structure of poly(diethylsiloxane) (PDES) has been characterized using solid-state NMR of (17)O. The sample studied had a weight-average molecular weight of 2.45 x 10(5). The sample was prepared by utilizing the cationic ring-opening polymerization of (17)O-enriched hexacyclotrisiloxane. Solid-state NMR of (17)O-enriched PDES was measured on the low-temperature beta(1) phase, the high-temperature beta(2) phase, the two-phase system consisting of the liquid crystal and isotropic liquid phase and the isotropic phase. From these data, the molecular structure and dynamics of PDES in the various phases were characterized via the chemical shifts of (17)O, and electric field gradient parameters were determined from NMR and ab initio molecular orbital (MO) calculations. In addition to the solid-state NMR of (1)H, (13)C and (29)Si previously reported on these samples, knowledge of the dynamic behavior of PDES as inferred from the NMR of (17)O in the present study was enhanced significantly. Further, the potential of combining the experimental NMR of (17)O with ab initio MO calculations to characterize the dynamics of polymers containing oxygen is demonstrated.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call