ZnO,CdO,ZnO-CdO nanocomposite were prepared using electrochemical deposition the prepared samples were characterized using X-ray diffraction and the photoluminenscence spectroscopy (PL) to get the surface morphology leading to calculation of optical energy gap .the grain size determined by Scherrer's equation (22-25) nm .through the calculation of Eg ,it was noticed a red shift behavior in ZnO manner due to addition of CdO content

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.