Undoped and silver, lithium and cobalt-doped ZnO thin films have been successfully deposited on glass by chemical bath deposition (CBD). The reaction temperature was 50∘C and the films were annealed at 400∘C for 4[Formula: see text]h in a high temperature furnace. UV/VIS spectrum was used to determine optical transmittance, optical band gap ([Formula: see text] and absorbance values of Ag:ZnO, Co:ZnO, Li:ZnO and undoped ZnO thin films. Optical band gap ([Formula: see text] and absorbance values of undoped ZnO, Ag:ZnO, Co:ZnO and Li:ZnO thin films were found as 0.0158, 0.0064, 0.2638, 0.0956 and 3.24, 3.13, 3.27, 2.96 eV, respectively. Extinction coefficients and refraction indexes of the films were found to be 0.0096, 0.0038, 0.0068, 0.019 (extinction coefficient) and 1.26, 1.14, 1.66, 2.33 (refraction index), respectively. X-ray patterns of undoped ZnO, Ag:ZnO, Co:ZnO and Li:ZnO thin films were confirmed as amorphous.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.